[meteorite-list] Nitric Acid / Ferric Chloride
ian macleod
ianmacca81 at hotmail.com
Thu Jun 26 02:47:55 EDT 2014
Hi Mendy
We have found that Nitric Acid produces a far better result than Fer-Chloride solution
What you may want to try is washing the slice after each etch with a alcohol solution, then etch again. Another modification is warming the etching solution (we have not tried this yet, but may produce better results)
A stir of the solution to agitate the processes like a washing machine does
Personally I would not combine the two, there maybe impurities that will react?
If washing is used between etching, different methods could be used safely
If you want to experiment with direct mixing, take 1 mol of each mix in a clean glass jar with some iron shavings like campo
cheers
Ian 8013